Database Materiali
24 Tutti · ricercabili
| Materiale | Famiglia | Resistenza (MPa) | Temp Stampa | Flessibilità | Resistenza UV | Fascia di Prezzo | |
|---|---|---|---|---|---|---|---|
| PLA High Speed | PLA (Acido polilattico) | 45 | 200–230°C | Rigido | Basso | Base | Confronta |
| PLA Matte | PLA (Acido polilattico) | 43 | 200–220°C | Rigido | Basso | Base | Confronta |
| PLA Silk | PLA (Acido polilattico) | 42 | 205–225°C | Rigido | Basso | Standard | Confronta |
| PETG Standard | PETG | 50 | 230–250°C | Medio | Medio | Standard | Confronta |
| PETG High Speed | PETG | 48 | 240–260°C | Medio | Medio | Standard | Confronta |
| ABS Standard | ABS (Plastica tecnica) | 44 | 230–260°C | Rigido | Basso | Standard | Confronta |
| ASA Standard | ASA (Resistente agli agenti atmosferici) | 45 | 240–260°C | Rigido | Alto | Standard | Confronta |
| TPU 95A | TPU (Elastomero) | 38 | 210–230°C | Flessibile | Basso | Premium | Confronta |
| PA-CF Nylon | PA (nailon) | 85 | 260–290°C | Rigido | Medio | Premium | Confronta |
| PC Standard | PC (Policarbonato) | 62 | 270–300°C | Rigido | Basso | Premium | Confronta |
| PVA Support | PVA / BVOH (Supporto solubile) | 30 | 200–220°C | Medio | Basso | Premium | Confronta |
| HIPS Support | HIPS (Supporto rimovibile) | 30 | 220–250°C | Rigido | Basso | Standard | Confronta |
| TPU 85A | TPU (Elastomero) | 30 | 200–230°C | Molto flessibile | Basso | Premium | Confronta |
| Multicolor | PLA (Acido polilattico) | 45 | 200–230°C | Rigido | Basso | Premium | Confronta |
| Rainbow | PLA (Acido polilattico) | 45 | 200–230°C | Rigido | Basso | Premium | Confronta |
| TPE | TPE | 25 | 210–230°C | Molto flessibile | Basso | Premium | Confronta |
| TPC | TPC | 35 | 220–250°C | Flessibile | Medio | Premium | Confronta |
| PVB | PVB | 40 | 190–220°C | Rigido | Basso | Standard | Confronta |
| PEI | PEI | 100 | 360–390°C | Rigido | Alto | Premium | Confronta |
| PEEK | PEEK | 100 | 380–420°C | Rigido | Alto | Premium | Confronta |
| PEKK | PEKK | 90 | 350–390°C | Rigido | Alto | Premium | Confronta |
| PVDF | PVDF | 50 | 240–260°C | Rigido | Alto | Premium | Confronta |
| PPSU | PPSU | 70 | 350–390°C | Rigido | Alto | Premium | Confronta |
| Resin | RESIN | 50 | — | Rigido | Medio | Premium | Confronta |